Blog

Laser-CMT Composite Welding: An Outstanding Solution for Ultra-Low Heat Input

Laser-CMT composite welding combines the high energy density of laser welding with the low heat input and controlled droplet transfer of Cold Metal Transfer (CMT) technology. By integrating these two processes, it offers improved control over the welding pool, heat distribution, and material transfer. This hybrid welding approach is particularly suitable for precision applications involving thin-walled structures, heat-sensitive materials, and components with stringent requirements for dimensional accuracy, joint quality, and surface integrity.

Technical Principle
Laser-CMT composite welding achieves a technological breakthrough through "cold-state welding + intelligent control". The CMT technology employs a current-free return mechanism to achieve ultra-low heat input (≤ 50 J/mm). At the same time, the laser keyhole and arc length closed-loop control (±0.01mm accuracy) work together to stabilize the molten pool, effectively avoiding the occurrence of incomplete fusion defects.

Core Advantages
Ultra-Low Heat Input: The CMT pulsed wire feeding technology results in a heat input of less than 8kJ/cm, which is 40% lower than traditional TIG welding. After welding 1.2mm titanium alloy plates, the angular deformation is less than 0.5°, significantly reducing the impact of welding deformation on the dimensional accuracy of the workpiece.

Droplet Control: No spatter short-circuit transition, dynamic stability of the molten pool, X-ray detection of porosity rate < 0.1%. Combined with the laser keyhole effect, the depth consistency error is less than 5%, ensuring the stability and consistency of the welding quality.

Efficiency Enhancement: The welding speed reaches 2.4m/min (equivalent heat input), doubling the efficiency of the CMT single-machine process, suitable for the welding of thin-walled components such as nuclear power main pipes, improving production efficiency.

Heat-Affected Zone Refinement: The grain size is reduced from 50μm to 15μm, with a 20% increase in mechanical properties, enhancing the strength and toughness of the welding joint.

Minimal Deformation: The angular deformation of 10mm thick plates is ≤ 0.5°/m, no need for subsequent correction, reducing production costs and cycle times.

Zero Spatter Forming: Reduces 80% of the grinding workload, the standard deviation of joint strength ≤ 5MPa, improving the appearance quality and performance stability of the product.

Application scenario
Suitable for high-precision component welding, such as the fuel tank of a space launch vehicle (10-25mm thick, deformation ≤ 0.1mm/m), semiconductor vacuum chambers (inner wall flatness ≤ 0.05mm), etc. In these fields, the requirements for welding deformation, heat affected zone and surface quality are extremely strict. The laser-CMT composite welding technology can achieve "ready-to-use after welding", meeting their high standards.

Tags: